View Single Post
Old 07-15-2013, 12:25 PM   #77
glatt
 
Join Date: Jul 2003
Location: Arlington, VA
Posts: 27,717
Quote:
Originally Posted by glatt View Post
Here's the finished boat. I was supposed to varnish it to protect the epoxy from UV rays, but I never did. It's stored in the dark, so it's been fine for the past 9 years.
Name:  kayak new.jpg
Views: 326
Size:  64.9 KB
It's been 3 years since I wrote that, and the kayak hasn't been treated kindly. Its storage location went from being under a cottage to under a deck. And snow melt got past the cockpit cover and filled the entire kayak, including behind the bulkheads, with water that year.

It's seen too much UV exposure, and lost much of its epoxy finish on the deck.
Name:  kayak deck 1.jpg
Views: 325
Size:  157.4 KB

A close up of the cockpit (with damaged cover in place) shows the real wear and tear on the deck. Lots of bare wood there.
Name:  kayak deck 2.jpg
Views: 319
Size:  117.8 KB
glatt is offline   Reply With Quote